InsuliserBeta
How the models work · Moisture model

6. Rain, ground moisture and cavities

Rain

During a shower, the rain on the wall is added to the outer slice. Capillary flow then draws it inward, as fast as the material's suction allows. Whatever the outer slice can't hold beyond its free saturation runs off at the end of the step. So a strongly wicking face takes up most of a shower, and a face with low A saturates in its outer millimetres and sheds the rest.

Ground moisture

Ground moisture reaches the run of layers from the outside that have capillary data, stopping at the first that doesn't (usually insulation). The model looks at the wall 1 m above the footing. It can't follow water rising from below, so while water stands at the footing (November to March for "wet in winter", all year for "wet all year"), each slice in that run is fed by capillary flow, worked out with the Kirchhoff potential, the integral of the liquid diffusivity, K(w) = ∫ Dw dw. The wall is saturated at the base and dry at the damp front, height h (below). In between, evaporation draws water off evenly with height, so the upward flow falls steadily to nothing at the front and the potential tapers as:

K(z) = K(wf) × (1 − z ÷ h)²

Because the liquid diffusivity rises steeply with water content, the wall stays fairly wet most of the way up and dries out close to the front. The slice at 1 m is fed towards the value at z = 1 m:

supply = [ K(1 m) − K(w) ] ÷ (h − 1 m)² per m³ of material

The distance h − 1 m is the gap over which the profile falls to nothing, so as the front comes down towards 1 m the supply settles at K(wf) ÷ h² rather than vanishing.

It only ever adds water: a slice wetter than that, from rain for instance, is not drained by the ground. It is strongest in materials that wick well.

How high the damp actually rises comes from sharp-front theory (Hall and Hoff). The wet zone, height h, is fed by capillary inflow at the base and dries through its faces at a rate e per square metre of wall. The tool follows it through the year:

d(h²)/dt = S² ÷ θ² − 2 e h² ÷ (θ b) settling at h = S × √( b ÷ (2 θ e) )

Here S is the sorptivity of the wicking run (its A divided by the density of water), b its thickness and θ its water content at free saturation as a volume fraction. The drying rate e comes from the simulation at every step: what the wicking run would lose through its outer face and into the layers behind it if it were wet, so it depends on the weather and the build-up. When the ground at the base dries, the inflow stops and the front falls. The tool reports the highest and lowest the front reaches over the year. With "wet in winter" the front starts low each November and climbs towards the winter height; with "wet all year" it stays up all year and is lowest in summer, when walls dry fastest. A render or insulation that slows drying lowers e and raises h. The slice at 1 m only receives rising damp once the front has climbed past it.

Saturated layers

A wicking material can only hold so much water in its pores: its free saturation. Water arriving beyond that, from heavy rain, ground moisture or condensation, can't be held, so it runs down out of the layer. The tool removes it at each step and reports it as water running down inside the wall. Layers with no storage data, such as foam boards and mineral wool, keep condensation as free water instead.

Cavities

Water that would collect in an air cavity beyond saturation is assumed to run down and out through the weep holes. It is counted as "drained" but not held. This assumes the cavity is clear and has working drainage, which is worth checking on site, especially in older walls where mortar droppings can block it. Condensation on a wicking cavity face, such as brick, soaks into that layer instead, and is held there.