Absorbent and wicking materials
Many traditional materials, such as wood fibre, cork, wool, timber, lime, clay, brick and stone, are hygroscopic: they take up moisture from damp air and give it back when the air dries. How much each holds at a given humidity is its sorption curve. The tool stores moisture in every layer along its own curve, so an absorbent layer buffers winter dampness instead of letting it collect as free water at a boundary.
Porous mineral materials also wick: liquid water moves through their fine pores by capillary suction, from wetter to drier, much faster than vapour can diffuse. How strongly is measured by the water absorption coefficient, A: the water a face soaks up from contact with water, in kg/m² per square root of time.
| Material | A, kg/(m²·s½) |
|---|---|
| Calcium silicate board | about 1 |
| Soft and stock brick | about 0.25–0.3 |
| Gypsum plaster and plasterboard | about 0.3 |
| Solid brick, porous limestone | about 0.15–0.2 |
| Lime render and plaster | about 0.06–0.08 |
| Lime-cement render | about 0.03 |
| Cement render, concrete | about 0.01–0.02 |
| Granite, foam boards, mineral wool | effectively 0 |
This is why a lime render behaves so differently from a cement one on an old solid wall, although their µ values are close. Water that gets into the brick behind a lime render is wicked back out to the face, where it evaporates. A cement render wicks so slowly that the water must leave as vapour, through a layer that resists it, so the brick behind it stays wetter for longer. No rule about "breathable" materials is involved: it follows from each material's A, its sorption curve and its µ.
For organic layers (wood fibre, cork, wool, hemp, cellulose, timber boards and similar) the tool also reports the peak moisture content, as a percentage of dry mass, averaged over the 10 mm at the layer's wetter face. It uses 18% as the limit, a cautious figure: about 20% is usually quoted for the onset of rot in timber. Mineral materials are not given a limit, because no single threshold fits their frost and salt risks.